304 Stainless Steel

Austenitic grade · UNS S30400 · EN 1.4301

Type 304 is a general-purpose chromium-nickel stainless grade chosen for its practical balance of corrosion resistance, forming performance, weldability, availability and cost.

It is commonly specified for food equipment, tanks, kitchen systems, architectural panels, appliances and fabricated industrial components. The material is a strong baseline choice for mild service, but chloride exposure, heavy welding and aggressive cleaning chemicals can change the correct grade selection.

Structure Austenitic
Common names 304 · SUS304 · 1.4301
Best fit General fabrication
Review another grade when Chlorides or heavy welding dominate
Stacked stainless steel sheets and plates in a warehouse
Stainless steel sheet and plate stock. Confirm the grade, heat number, thickness, finish and inspection documents for each order.

When 304 Is the Right Grade—and When It Is Not

Usually a good starting choice

  • Indoor equipment and architectural components.
  • Food, beverage and kitchen equipment with suitable cleaning practices.
  • Fresh-water systems and many mild industrial environments.
  • Sheet-metal parts requiring bending, drawing, stamping or welding.
  • Projects that need broad global availability in sheet, coil, tube or bar.

Review another grade before ordering

  • Coastal, marine, swimming-pool, brine or chloride-cleaning exposure.
  • Thick welded sections where sensitization resistance is important.
  • Strong acids, concentrated chemicals or high process temperatures.
  • Projects requiring higher strength with lower section thickness.
  • Specifications that mandate a low-carbon, stabilized or duplex grade.

For welded fabrication in mild service, compare 304L. For chloride-bearing environments, review 316L, 2205 duplex or 2507 super duplex according to the actual concentration, temperature, design and maintenance conditions.

304 Stainless Steel Supply: Choose the Product Form

304 is supplied in several product forms, but each uses different standards and acceptance checks. Choose the relevant product page before requesting a price.

304 Sheet / Plate

Thickness, width, length, 2B or No.1 finish, flatness and film.

Sheet and plate options →
304 Coil / Strip

Width, temper, thickness, edge, coil ID, coil weight and finish.

Coil supply options →
304 Pipe / Tube

Seamless or welded route, OD, wall, length, inspection and finish.

Pipe and tube options →
304 Round / Flat Bar

Diameter or section, condition, tolerance, length and testing.

Bar supply options →

Example only: Type 304 / UNS S30400 sheet, ASTM A240, 1.50 × 1219 × 2438 mm, 2B, tolerance per agreed standard, required quantity, MTC, delivery destination. This is a specification example, not confirmed stock or a price offer.

Standards and Equivalent Grade References

This alloy appears under several national and international designations. These names are useful for cross-reference, but they should not be treated as automatic substitutes. Final acceptance must follow the standard edition, product form and test requirements stated on the purchase order and mill test certificate.

Common 304 grade designations
Country / regionReference systemDesignationProcurement note
InternationalUNSS30400Widely used as the unified alloy designation.
United StatesAISI / SAE304Commercial grade name; specify the applicable product standard.
United StatesASTM A240 / A276 / A312 / A479 / A666Type 304 / S30400The relevant standard depends on sheet, plate, bar, pipe or strip.
EuropeEN 100881.4301 / X5CrNi18-10Check the relevant EN product standard and delivery condition.
JapanJIS G 4303 / G 4304 / G 4305SUS304Product form and dimensional standard still need confirmation.
ChinaGB/T 20878 reference06Cr19Ni10Use the applicable GB product standard for final acceptance.
Russia / CISCommon GOST cross-reference08Х18Н10Commonly compared in the market; chemistry and specification must be verified.

Data-use note: standard numbers and grade cross-references are provided for specification review. Always use the edition and product standard named in the contract. See the stainless steel grades overview for the wider grade family.

Chemical Composition

Chromium forms the passive film responsible for stainless behavior, while nickel supports the austenitic structure, toughness and forming performance. The table below summarizes commonly specified limits for Type 304; these figures are a flat-product specification reference, not a heat analysis. The ordered standard and its edition govern.

Type 304 / UNS S30400: indicative ASTM A240 flat-product limits (wt.%)
ElementCommonly specified limitWhy it matters
Carbon (C)≤ 0.08%Affects strength and sensitization behavior after thermal exposure.
Chromium (Cr)18.00–20.00%Supports the passive film and oxidation resistance.
Nickel (Ni)8.00–10.50%Stabilizes austenite and supports ductility and toughness.
Manganese (Mn)≤ 2.00%Supports steelmaking control and austenite stability.
Silicon (Si)≤ 0.75%ASTM flat-product reference; other standards may set different limits.
Nitrogen (N)≤ 0.10%Can contribute to strength and austenite stability.
Phosphorus (P)≤ 0.045%Controlled residual element.
Sulfur (S)≤ 0.030%Controlled for ductility, surface quality and corrosion performance.
Iron (Fe)BalanceBase metal.

Do not approve a shipment from a grade name alone. Match the heat number on the material marking to the heat number and chemistry shown on the mill certificate.

Mechanical and Physical Properties

Mechanical properties in annealed condition

Type 304 is not hardened by quenching. Cold rolling, drawing and forming can raise strength and hardness while reducing ductility. Because requirements change by thickness, product form and test direction, the purchase specification remains the controlling document.

Indicative room-temperature specified minima for the stated flat-product standards
Product form / referenceTensile strength0.2% yield strengthElongationHardness note
ASTM A240 sheet / plate, annealed≥ 515 MPa≥ 205 MPa≥ 40%Common maximum: 201 HBW
EN 1.4301 sheet / plate, annealedCommon reference: ≥ 520 MPaCommon reference: ≥ 210 MPaCommon reference: ≥ 45%Depends on thickness and product standard
JIS SUS304 sheet / strip, annealedCommon reference: ≥ 520 MPaCommon reference: ≥ 205 MPaCommon reference: ≥ 40%Confirm the applicable JIS requirement
Cold-worked strip or drawn productHigher than annealed materialHigher than annealed materialLower than annealed materialControlled by temper and reduction

Physical-property reference values

Typical physical data for engineering estimates
PropertyReference valueUse note
DensityApproximately 7.9–8.0 g/cm³Use the project value for precision weight calculations.
Melting rangeApproximately 1390–1450°CNot a recommended service-temperature limit.
Elastic modulusApproximately 190–200 GPaVaries with temperature and reference source.
Thermal conductivityApproximately 16 W/(m·K) near 100°CLower than carbon steel; consider this during welding and heating.
Electrical resistivityApproximately 0.72 μΩ·mReference value, temperature dependent.
Magnetic responseUsually low when solution annealedCold work can produce noticeable magnetic attraction.

Corrosion Resistance, Welding, Forming and Machining

Corrosion behavior

The grade performs well in many atmospheric, indoor, food, fresh-water and mild process environments. Deposits, chloride cleaners, stagnant water and iron contamination can still cause staining or localized attack.

Welding and heat tint

Common stainless welding processes can be used. Remove heat tint and contamination when corrosion performance matters. For extensive welding or thicker sections, compare the low-carbon 304L variant.

Forming and work hardening

The material bends and deep draws well, but it work-hardens during deformation. Tooling, intermediate annealing and forming sequence should be reviewed for severe reductions.

Fabrication and service checks before release
CheckPractical implicationCommon buyer action
Chloride exposureRisk increases with concentration, temperature, deposits, crevices and poor drainage.Share the medium, temperature and cleaning method before grade approval.
Welded constructionHeat tint and sensitization-related concerns can reduce local corrosion performance.Review 304L, welding procedure, cleaning and passivation requirements.
MachiningWork hardening and poor chip control can shorten tool life.Use rigid setups, sharp tools, positive feeds and suitable coolant.
Decorative finishGrain direction, gloss, film and handling determine visual acceptance.Approve samples and specify the visible side and film type.
Food or hygienic useGrade alone does not guarantee hygienic performance.Confirm finish, weld quality, drainage, cleaning regime and local regulations.

Why Received 304 Material May Show Slight Magnetism

A frequent receiving-inspection question is: “The certificate says 304, so why does a magnet still attract the edge or bent area?” Austenitic material can develop deformation-induced martensite during cold rolling, bending, stamping, drawing or machining. The magnetic response is often strongest at worked edges and corners rather than across a fully annealed flat surface.

A magnet is therefore a quick screening tool, not a definitive grade-verification method. Use the heat number, MTC and—when the project risk justifies it—PMI/XRF or laboratory analysis. Note that handheld XRF does not directly measure carbon, so it cannot by itself distinguish every low-carbon grade question.

Practical warning: do not reject or approve a heat solely from magnetic attraction. Review the location tested, amount of cold work, certificate traceability and chemical-verification method.

Inspection, Traceability and Documents Buyers Should Request

For specification-controlled orders, use a documented material-receiving and inspection process. Agree which records and tests are required before dispatch.

Heat-number match

Check that material markings, bundle tags and MTC heat numbers correspond.

MTC review

Confirm grade, standard, chemistry, mechanical results, dimensions and delivery condition.

Dimensional check

Measure thickness, width, length, flatness or tube dimensions against the purchase order.

Surface inspection

Check finish, scratches, edge condition, grain direction, film and visible-side marking.

Useful order and inspection documents
Document / checkWhat it should confirmWhen it matters most
Mill test certificateHeat number, chemistry, mechanical properties and specification.Every specification-controlled export order.
PMI / XRF reportAlloy-family screening and selected elemental verification.Mixed-stock risk, critical fabrication or end-user requirement.
Dimensional reportThickness, width, length, diameter, wall thickness or tolerance.Tight-tolerance processing and drawing-based parts.
Surface / packing photosFinish, film, labels, pallet or crate condition before shipment.Decorative products and export logistics.
Third-party inspectionIndependent witness or verification against the agreed scope.Projects with contractual inspection points.

Typical Applications and Selection Risks

Food and kitchen equipment

Worktables, sinks, covers, tanks, conveyors and appliances where finish, cleaning and weld quality are controlled.

Architecture and interiors

Panels, doors, trims, handrails and visible components using 2B, BA, No.4, hairline or mirror finishes.

General industrial fabrication

Machine guards, frames, brackets, water-system parts, light process equipment and custom-cut components.

Four common specification mistakes

  1. Using “18-8” as the complete specification. It is a broad market description, not a substitute for a product standard, dimensions and test requirements.
  2. Choosing the grade before reviewing chlorides. Coastal deposits, salt, pool chemicals and chloride cleaners can make 316L or duplex material more appropriate.
  3. Ignoring fabrication condition. Heavy welding, cold work, heat tint and embedded iron can change local corrosion behavior.
  4. Ordering a finish name without an approval basis. No.4, hairline and mirror appearance can vary by abrasive route, grain, gloss, film and base surface.

304 Compared with 201, 303, 304L, 316L, 430 and 2205

The correct alternative depends on why the buyer is moving away from 304: lower cost, better machining, improved post-weld performance, stronger chloride resistance, magnetic behavior or higher strength.

Fast material-selection comparison
GradePrimary reason to choose itMain trade-off or checkTypical decision context
304Broad all-round balance and availability.Not the default choice for severe chlorides or heavy welded corrosion service.General fabrication, kitchen equipment, tanks and panels.
201Lower alloy cost for selected mild indoor applications.Corrosion behavior and market acceptance must be reviewed.Cost-sensitive decorative and appliance parts.
303Improved machining and chip control.Reduced corrosion performance and limited welding suitability.High-volume machined fittings, shafts and fasteners.
304LLow carbon for welded fabrication.Confirm whether the design requires standard 304 strength or dual certification.Welded tanks, pipework and thicker sections.
316LBetter resistance to many chloride and process environments.Higher alloy cost; still not immune to severe seawater attack.Coastal, chemical, food and pharmaceutical systems.
430Ferritic, magnetic grade with little intentional nickel addition.Lower formability, weldability and corrosion performance in many services.Dry indoor appliance and decorative components.
2205Higher strength and stronger chloride resistance.Requires duplex-specific fabrication and welding control.Pressure equipment, chemical tanks, brine and chloride service.

Product Forms, Surface Finishes and Processing

Stainless steel round tubes prepared for industrial supply
Pipe and tube orders should state the standard, OD, wall thickness, length, end condition, surface and testing scope.
Stainless steel coils with protective wrapping stored for processing
Coil orders should also confirm coil ID, coil weight, edge condition, surface film and processing route.
Available supply routes
Product or serviceKey RFQ informationUseful page
Sheet / plateThickness, width, length, finish, tolerance, visible side and film.Sheet / plate supply
Coil / stripThickness, width, coil ID, coil weight, edge, temper, finish and film.Coil supply
Pipe / tubeStandard, OD, wall thickness, length, welded or seamless, finish and testing.Pipe / tube supply
Bar and long productsShape, diameter or section, length, tolerance, condition and testing.Flat / round bar
Cut-to-length and slittingFinished dimensions, tolerance, burr, flatness, coil plan and packing quantity.Cut-to-length / slitting
Surface finishingBase finish, target finish, grain direction, sample, gloss and protective film.Surface finishing
Laser / waterjet cuttingDrawing, material thickness, tolerance, edge requirement and part quantity.Laser cutting

Information Needed for an Accurate Quotation

MOQ, stock availability and lead time cannot be stated accurately without the product form and specification. A complete RFQ lets the supplier distinguish stock material from mill production and identify the processing route before quoting.

  • Grade and standard: 304 / S30400 / SUS304 / 1.4301, plus the applicable ASTM, EN, JIS or GB product standard.
  • Product form and dimensions: sheet, plate, coil, strip, pipe, tube or bar with full sizes and tolerances.
  • Surface and processing: No.1, 2B, BA, No.4, HL, mirror, cutting, slitting, polishing or film.
  • Quantity: total weight, number of pieces, coil weight or bundle quantity.
  • Inspection scope: MTC, PMI, dimensional report, third-party inspection or project-specific testing.
  • Commercial details: destination port, Incoterm, packing requirement and requested delivery window.

For China-origin quotations, confirm whether the offer is from available stock, scheduled mill production or processing to order. MOQ, delivery and documentation depend on the exact specification.

Practical Questions Buyers Ask About 304

Why does a supposedly non-magnetic 304 sheet attract a magnet after bending?

Cold rolling, bending, stamping and machining can transform part of the austenitic structure and increase magnetic response. Attraction concentrated at worked edges or bends is not, by itself, proof that the material is the wrong grade.

Can a magnet test distinguish 201 from 304?

No. Magnetic response depends on composition, annealing and cold work. Verify the heat number and MTC, then use an appropriate chemical-analysis method when independent confirmation is required.

Why can 304 develop brown stains even when the certificate is correct?

Possible causes include embedded carbon-steel particles, chloride deposits, poor drainage, heat tint, damaged passive film or unsuitable cleaning chemicals. The location and pattern of staining should be inspected before concluding that the alloy chemistry is wrong.

When should a welded project specify 304L instead?

304L is commonly reviewed when the fabrication contains extensive welding, thicker sections or corrosion-sensitive heat-affected zones. The design code and required mechanical properties should determine the final choice.

Is 304 suitable for coastal, pool or salt-water equipment?

It should not be treated as the default choice. Chloride concentration, temperature, deposits, crevices, cleaning and maintenance all affect risk. 316L or a duplex grade may be more suitable after technical review.

What should be checked on a 304 mill test certificate?

Check the supplier and mill, heat number, grade designation, applicable standard, chemistry, mechanical results, product dimensions and delivery condition. The heat number should match the material or bundle identification.

Which finish is better for kitchen equipment: 2B, No.4 or hairline?

2B is a common industrial base finish. No.4 provides a practical brushed appearance that can hide minor handling marks, while hairline gives a longer directional grain for decorative panels. Cleaning method, visible side, grain direction and protective film should be specified.

Technical References and Specification Limits

Material information above is for initial grade selection. Exact acceptance limits depend on the applicable edition, product form and order conditions. Do not treat an indicative physical-property value as a guaranteed mill result.

Technical review note: this page is a procurement and material-selection guide, not a substitute for the project code, current standard edition, corrosion study or engineer approval. Final acceptance should follow the purchase specification and verified inspection documents.

Request a 304 Stainless Steel Quotation

Send the grade and standard, product form, full dimensions, surface finish, quantity, processing, inspection scope and destination port. XRTGSteel can then check current stock, mill production, MOQ, processing route, packing and lead time for the exact requirement.

300

Does 304 Stainless Steel Rust?

304 is highly resistant to rust, but it is not rust-proof. It stays stainless because a thin, chromium-rich passive film forms on its surface and repairs itself in air. Rust appears when that film is broken down locally faster than it can repair, or when iron from another source is left on the surface.

Why 304 Stainless Steel Rusts: The Common Causes

CauseWhat you seeTypical situation
Chlorides (pitting and crevice corrosion)Small pits or rust spots, often under deposits or in gapsCoastal air, de-icing salt, swimming pools, bleach or chloride cleaners
Tea stainingLight brown surface discolorationOutdoor surfaces within a few kilometres of the sea, rough finishes, areas not washed by rain
Free-iron contaminationOrange rust specks that appear soon after fabricationCarbon-steel tools, wire brushes, grinding dust or storage next to carbon steel
Weld heat tintStraw-to-blue oxide colours with rust along the weldWelds not pickled or passivated after welding
SensitizationCorrosion along grain boundaries near weldsStandard-carbon 304 held in about 425–815 °C, or heavy welding; 304L reduces the risk

How to Prevent and Remove Rust on 304

  • Avoid contamination: use stainless-only tools, brushes and abrasives, and store stainless separately from carbon steel.
  • Clean up after fabrication: remove heat tint and embedded iron by pickling, then passivate. ASTM A380 covers cleaning and descaling, and ASTM A967 covers chemical passivation treatments (nitric or citric acid).
  • Choose a smoother finish outdoors: a finer polish (lower Ra) holds fewer deposits and resists tea staining better than a coarse brushed finish.
  • Design for drainage: avoid crevices and water traps, and let rain wash exposed surfaces.
  • Clean regularly: wash with fresh water and a mild detergent, and do not use chloride bleach.
  • Upgrade the grade when chlorides are severe: use 316L (2–3% molybdenum) or a duplex grade for coastal, pool or salt-exposed applications.

Light rust staining can usually be removed with a non-scratch pad and a stainless cleaner based on oxalic or phosphoric acid, followed by rinsing. Deep pits mean the grade or design is wrong for the environment.

More 304 Questions

Will 304 stainless steel rust in saltwater?

Yes, it is likely to. 304 has no molybdenum, and seawater and salt spray cause pitting and crevice corrosion. It is not recommended for immersion in seawater. 316L handles occasional splash and coastal air better, and super duplex or 6Mo grades are used for seawater service.

Why does 304 stainless steel rust after welding?

Usually because of heat tint and iron contamination left on the weld. Pickling and passivating the weld area restores the passive film. For heavy sections or repeated welding, 304L is preferred over 304.

What gauge is 304 stainless steel?

304 is a grade, not a thickness. It is supplied in every common gauge and metric thickness, from thin foil-like strip to heavy plate. See our 304 stainless steel sheet thickness chart for gauge-to-mm conversions.