310S stainless steel is a high-alloy heat-resistant austenitic stainless steel. It contains high chromium and high nickel. As a result, it offers excellent oxidation resistance in many high-temperature environments.
This grade is the low-carbon version of 310 stainless steel. Therefore, it offers better weldability than higher-carbon 310 material. It is often used for furnace parts, radiant tubes, retorts, hot gas ducts and heat-treatment fixtures.
Compared with 309S stainless steel, 310S stainless steel gives stronger oxidation resistance. However, 310H stainless steel is often preferred when higher hot strength is required.
XRTGSteel supplies 310S stainless steel in sheet, plate, coil, strip, pipe, tube and bar. In addition, we provide slitting, cut-to-length, laser cutting, surface finishing, sawing and export packing.
What Is 310S Stainless Steel?
Basic Grade Definition
310S stainless steel is a 25Cr-20Ni heat-resistant stainless steel. Its high alloy content helps resist oxidation and scaling. For this reason, it is widely used in hot-service equipment.
Main Performance Advantage
The main advantage of 310S is heat resistance. It performs better than 304H stainless steel and 309S in many oxidizing atmospheres. Moreover, it keeps good toughness after proper solution annealing.
Common Supply Forms
XRTGSteel can supply 310S stainless steel sheet, plate, coil, strip, pipe, tube and bar. We can also prepare custom-cut parts according to drawings. This helps buyers reduce processing work before fabrication.
Standards & Equivalent Grades of 310S Stainless Steel
International Grade References
310S stainless steel is available under several international standards. However, equivalent grades are not always exact matches. Therefore, the purchase standard and MTC should be checked before production.
| Country / Region | Standard | Grade / Designation |
|---|---|---|
| International | UNS | S31008 |
| USA | AISI / SAE | 310S |
| USA | ASTM A240 / A312 / A276 / A479 | Type 310S |
| Europe | EN 10095 / EN 10088 | 1.4845 / X8CrNi25-21 |
| Japan | JIS | SUS310S |
| China | GB Reference | 06Cr25Ni20 |
| Common Name | Market Name | SS 310S / 25Cr-20Ni Stainless Steel |
Grade Selection Note
For high-temperature projects, buyers should confirm the service temperature, atmosphere and exposure time. In addition, the required inspection documents should be confirmed before shipment. More grades are listed in our stainless steel grades overview.
Chemical Composition of 310S Stainless Steel
Main Alloying Elements
Chromium and nickel are the key alloying elements in 310S stainless steel. Chromium improves oxidation resistance. Meanwhile, nickel helps maintain the austenitic structure at high temperature.
| Element | Typical Content | Main Function |
|---|---|---|
| C | ≤ 0.08% | Improves weldability through lower carbon control. |
| Cr | 24.00 – 26.00% | Provides oxidation and scaling resistance. |
| Ni | 19.00 – 22.00% | Supports austenite stability and toughness. |
| Mn | ≤ 2.00% | Supports steelmaking control. |
| Si | ≤ 1.50% | Supports oxidation resistance and deoxidation. |
| P | ≤ 0.045% | Controlled residual element. |
| S | ≤ 0.030% | Controlled for ductility and hot workability. |
| Fe | Balance | Main base metal. |
Composition Check Before Order
Chemical limits can change slightly by standard. Therefore, final acceptance should follow the order standard and the mill test certificate. XRTGSteel can supply MTC documents for export orders.
Mechanical Properties of 310S Stainless Steel
Room-Temperature Properties
310S stainless steel offers good strength and ductility after solution annealing. However, its main value is high-temperature oxidation resistance. For pressure service, the design code should always be reviewed.
| Product Form / Condition | Tensile Strength | Yield Strength | Elongation | Hardness |
|---|---|---|---|---|
| Annealed sheet / plate | ≥ 515 MPa | ≥ 205 MPa | ≥ 40% | ≤ 192 HBW typical |
| Annealed coil / strip | 515 – 760 MPa typical | 205 – 380 MPa typical | 35 – 45% typical | Depends on temper |
| Pipe / tube | 515 – 760 MPa typical | 205 – 380 MPa typical | 35 – 45% typical | Depends on wall thickness |
| Round bar / forged bar | 515 – 780 MPa typical | 205 – 400 MPa typical | 30 – 45% typical | Depends on size |
High-Temperature Design Note
High-temperature performance depends on temperature, atmosphere and load. In addition, continuous exposure and thermal cycling can affect service life. For critical equipment, allowable stress data should follow the project code.
Physical Properties of 310S Stainless Steel
Typical Physical Data
The physical properties of 310S stainless steel support heat-resistant applications. The grade is usually non-magnetic after solution annealing. After cold work, slight magnetism may appear.
| Property | Typical Value |
|---|---|
| Density | About 7.90 – 8.00 g/cm³ |
| Melting Range | About 1390 – 1450°C |
| Elastic Modulus | About 190 – 200 GPa |
| Thermal Conductivity | About 14 – 16 W/m·K at 100°C |
| Electrical Resistivity | About 0.78 μΩ·m typical |
| Magnetism | Generally non-magnetic when annealed |
Practical Service Note
Physical data should not be used alone for material selection. Instead, temperature, atmosphere and mechanical load should be reviewed together. This approach helps avoid early failure in hot-service components.
Key Features of 310S Stainless Steel
Performance Highlights
310S stainless steel is chosen for severe heat exposure. It offers a strong balance of oxidation resistance, weldability and fabrication performance. In addition, it is available in many product forms.
Excellent Oxidation Resistance
High chromium helps 310S resist scaling in many hot oxidizing atmospheres.
High Nickel Stability
High nickel supports austenite stability and toughness at elevated temperatures.
Low-Carbon Weldability
Lower carbon improves weldability compared with higher-carbon 310 material.
Summary of Advantages
- High-alloy heat-resistant austenitic stainless steel.
- Excellent oxidation resistance in many hot oxidizing atmospheres.
- Better heat resistance than 309S and 304H in many applications.
- Good weldability because of lower carbon content.
- Good ductility and formability after solution annealing.
- Available as sheet, plate, coil, strip, pipe, tube and bar.
- Suitable for furnace parts, radiant tubes, fixtures and hot ducting.
- Needs technical review in reducing, carburizing or sulfur-bearing atmospheres.
Heat Resistance, Oxidation Resistance and Weldability
Oxidizing Atmospheres
310S stainless steel performs best in oxidizing high-temperature atmospheres. Because of its high chromium level, it forms a protective oxide scale. As a result, it resists scaling better than many 300-series grades.
Special Atmospheres
Some hot atmospheres are more difficult. For example, carburizing, nitriding, reducing or sulfur-bearing gases may reduce performance. Therefore, gas chemistry should be reviewed before final material selection.
Welding and Fabrication
310S stainless steel can be welded by common stainless steel methods. However, filler selection and heat input control remain important. After welding, cleaning helps protect surface quality and corrosion resistance.
| Performance Item | 310S Stainless Steel Characteristics |
|---|---|
| Oxidation Resistance | Excellent in many oxidizing high-temperature atmospheres. |
| Scaling Resistance | Stronger than 309S and 304H in many hot-service conditions. |
| Weldability | Good because of low carbon content. |
| Formability | Good after solution annealing and with suitable tooling. |
| Heat Treatment | Not hardenable by quenching. |
| Surface Finish | Available in No.1, 2B, BA, No.4 and polished finishes. |
Typical Applications of 310S Stainless Steel
Furnace and Heat-Treatment Equipment
310S stainless steel is widely used in furnace systems. Common parts include furnace liners, radiant tubes, muffles, retorts and burner components. In addition, it is used for trays, baskets, jigs and heat-treatment fixtures.
Hot Gas and Thermal Processing Systems
Hot gas systems often need strong oxidation resistance. Therefore, 310S is used for ducting, stacks, chimneys and exhaust parts. It is also used in kilns, dryers, thermal enclosures and combustion chambers.
Refinery and Industrial Equipment
Refineries and petrochemical plants use 310S for suitable high-temperature parts. Typical examples include heater components, shields, transition pieces and thermal processing assemblies. However, the medium and atmosphere must be checked first.
- Furnace liners, doors, supports and internals.
- Radiant tubes, retorts, muffles and burner parts.
- Heat-treatment trays, baskets, jigs and fixtures.
- High-temperature ducts, stacks, chimneys and flue gas parts.
- Kiln components, dryer parts and thermal enclosures.
- Refinery heaters, shields and transition pieces.
- Heat exchangers, recuperators and baffles.
- Combustion chambers and hot gas manifolds.
310S vs 309S, 310H, 304H, 316H, 321, 347 and 446 Stainless Steel
Quick Comparison
Buyers often compare 310S with other heat-resistant grades. Each grade has a different balance of oxidation resistance, hot strength, cost and weldability. Therefore, the service condition should guide the final choice.
| Grade | Main Advantage | Typical Use |
|---|---|---|
| 310S | Excellent oxidation resistance and good weldability. | Furnace parts, radiant tubes and hot ducting. |
| 309S | Good heat resistance with lower alloy cost. | Furnace fixtures and thermal parts. |
| 310H | Higher hot strength than 310S. | High-strength furnace and pressure parts. |
| 304H | 304-family high-temperature strength. | Boilers and hot process piping. |
| 316H | Hot strength plus molybdenum-bearing corrosion resistance. | Heat exchangers and process equipment. |
| 321 / 347 | Stabilized performance for selected thermal service. | Expansion joints and welded hot parts. |
| 446 | High-chromium ferritic oxidation resistance. | Burners and combustion chambers. |
Selection Guidance
- Choose 310S for severe oxidation resistance and good weldability.
- Choose 309S when the full performance of 310S is not required.
- Choose 310H when higher hot strength is important.
- Choose 304H for many 304-family high-temperature pressure parts.
- Choose 316H when molybdenum-bearing corrosion resistance is also needed.
- Choose 321 or 347 when stabilized stainless steel is required.
- Choose 446 when a ferritic heat-resistant grade is suitable.
310S Stainless Steel Product Forms
Sheet, Plate and Coil
XRTGSteel supplies 310S sheet, plate and coil for furnace and heat-resistant fabrication. These products can be cut, slit, polished or packed according to the order.
| Product Form | Available Options | Typical Use |
|---|---|---|
| 310S Sheet / Plate | Hot-rolled plate, cold-rolled sheet and cut plate. | Furnace liners, heat shields and thermal panels. |
| 310S Coil | No.1, 2B, BA, No.4 and custom coil weight. | Cut-to-length, slitting and formed parts. |
| 310S Strip | Narrow strip and custom width strip. | Heat-treatment fixtures and formed parts. |
Pipe, Tube and Bar
Pipe, tube and bar are common choices for thermal equipment. For example, they are used in radiant tubes, supports, fixtures and machined parts.
| Product Form | Available Options | Typical Use |
|---|---|---|
| 310S Pipe / Tube | Seamless pipe, welded pipe and radiant tube. | Hot gas ducting and heat-resistant lines. |
| 310S Bar | Round bar, flat bar, forged bar and angle. | Supports, fixtures, fasteners and fittings. |
Processing and Testing Support
Processing Services
XRTGSteel can process 310S stainless steel before shipment. This helps buyers save time and control fabrication cost. Available services include cutting, slitting, surface finishing and sawing.
| Service | What We Provide |
|---|---|
| Cut-to-Length | Cut coil into sheets with required length and packing quantity. |
| Slitting | Slit coil into narrow strip for forming and fabrication. |
| Surface Finishing | Supply No.1, 2B, BA, No.4 and polished finishes. |
| Laser Cutting | Prepare blanks, heat shields and custom parts. |
| Saw Cutting | Cut bar, pipe and tube to required length. |
| Export Packing | Use waterproof paper, pallets, wooden cases and bundle protection. |
Inspection Support
For critical projects, we can coordinate PMI, tensile testing, hardness testing and third-party inspection. In addition, we can supply MTC documents and packing records.
How to Order 310S Stainless Steel from XRTGSteel
Information Needed for Quotation
A clear inquiry helps us quote faster. Please send the grade, size, quantity, surface finish and delivery destination. For heat-service projects, service conditions are also important.
- Grade: 310S, UNS S31008, 1.4845, SUS310S or 06Cr25Ni20.
- Product form: sheet, plate, coil, strip, pipe, tube, bar or custom part.
- Size: thickness, width, length, diameter or wall thickness.
- Surface finish: No.1, 2B, BA, No.4, polished or pickled.
- Processing: slitting, cutting, laser cutting, sawing or polishing.
- Service condition: temperature, atmosphere and exposure time.
- Testing requirement: MTC, PMI, tensile test or third-party inspection.
- Quantity: pieces, kilograms, tons, coil weight or bundle quantity.
- Delivery term: FOB, CFR, CIF, DDP or other agreed Incoterms.
Material Selection Support
If the best grade is not clear, send your drawing and service condition. Our team can compare 310S with 309S, 310H, 304H, 316H, 321, 347 and 446. Therefore, you can choose a safer material before ordering.
FAQ – 310S Stainless Steel
Q1: What is 310S stainless steel?
310S stainless steel is a high-alloy heat-resistant austenitic stainless steel. It contains high chromium and high nickel. Therefore, it offers excellent oxidation resistance in many hot environments.
Q2: What is the UNS number of 310S stainless steel?
The UNS number is S31008. Common equivalent names include AISI 310S, EN 1.4845, X8CrNi25-21, SUS310S and 06Cr25Ni20.
Q3: What is the difference between 310 and 310S stainless steel?
310S is the lower-carbon version of 310 stainless steel. Because of the lower carbon level, 310S offers better weldability.
Q4: What is the difference between 310S and 309S stainless steel?
310S has higher chromium and nickel than 309S. As a result, it usually gives better oxidation resistance at higher temperatures.
Q5: What is the difference between 310S and 310H stainless steel?
310S has lower carbon and better weldability. However, 310H has higher hot strength and better creep resistance.
Q6: Can 310S stainless steel be welded?
Yes. 310S stainless steel has good weldability. However, correct filler selection and heat input control are important for critical parts.
Q7: Is 310S stainless steel suitable for all high-temperature atmospheres?
No. 310S performs best in oxidizing atmospheres. Reducing, sulfur-bearing or carburizing atmospheres need separate technical review.
Q8: What 310S products can XRTGSteel supply?
XRTGSteel supplies 310S sheet, plate, coil, strip, pipe, tube and bar. We also provide cutting, slitting, finishing, sawing, testing support and export packing.
Request 310S Stainless Steel Price
Send your 310S stainless steel grade, product form, size, finish, quantity and destination port. XRTGSteel will help you confirm the right supply form and processing route.
For furnace, radiant tube, kiln, refinery or hot gas ducting projects, please also send the service temperature and atmosphere. This information helps us compare 310S with 309S, 310H, 304H, 316H, 321, 347 and 446 before quotation.