316Ti Stainless Steel

Titanium-stabilized Cr-Ni-Mo grade · UNS S31635 · EN 1.4571

Type 316Ti is a titanium-stabilized member of the 316 family. It retains molybdenum-assisted pitting resistance while using titanium to reduce chromium-carbide sensitization during suitable elevated-temperature exposure.

The grade is commonly reviewed for chemical plant equipment, refinery components, heat exchangers, hot process piping and fabricated parts that may remain in a sensitizing temperature range. Titanium stabilization does not make the alloy immune to seawater pitting, chloride stress-corrosion cracking, knife-line attack or incorrect heat treatment.

StructureAustenitic
Common names316Ti · S31635 · 1.4571
Defining featureTi stabilization
Selection contextSpecified stabilized service

Request a 316Ti Quote →

Representative stainless steel sheet and plate stock; 316Ti grade requires heat-specific documentation
Representative stainless sheet and plate stock, not a verified photograph of 316Ti material. Match the actual heat number to the MTC and confirm the specified S31635 or 1.4571 chemistry, delivery condition and product standard.

When 316Ti Is the Right Grade—and When It Is Not

Usually a good candidate for review

  • A specification explicitly requires UNS S31635, Type 316Ti or EN 1.4571.
  • Fabricated chemical or petrochemical equipment will experience prolonged or repeated thermal exposure.
  • 316-type molybdenum corrosion resistance is required together with titanium stabilization.
  • Heat exchangers, hot process lines, refinery parts or furnace-adjacent components require a stabilized austenitic grade.
  • The buyer can define the operating temperature, exposure time, corrosion medium and applicable design code.

Review another grade before ordering

  • The component is mainly welded at moderate temperature and low carbon is the project’s primary requirement.
  • High creep or stress-rupture strength is required but no elevated-temperature design data have been specified.
  • Warm, stagnant seawater, deposits, tight crevices or severe chloride stress-corrosion cracking risk dominate the service.
  • A highly polished, electropolished or pharmaceutical surface must meet strict cosmetic and inclusion limits.
  • The material will be exposed to strongly oxidizing acids where molybdenum-bearing stabilized grades require separate corrosion review.

Compare 316L for low-carbon welded corrosive service, 316H where controlled elevated-temperature strength is required, 321 for titanium-stabilized 18Cr-8Ni service without molybdenum, and 347 where niobium stabilization is specified. For stronger chloride and SCC resistance, review 2205 duplex or 2507 super duplex.

Standards and Equivalent Grade References

316Ti is represented by several international designations. These are useful cross-references, not permission to substitute without checking chemistry, product form, dimensions, solution treatment, stabilization requirements, mechanical properties and corrosion testing.

Common 316Ti designations and product-standard references
SystemDesignationTypical product referenceProcurement note
UNSS31635Unified alloy designationUse this designation when the ASTM/ASME specification recognizes 316Ti.
AISI / commercial316TiGeneral market nameAdd the applicable ASTM, ASME, EN or project product standard.
ASTM flat productsType 316Ti / S31635ASTM A240 / A480Confirm plate, sheet or strip thickness, finish and heat-treatment condition.
ASTM pipe / tubeTP316Ti / S31635ASTM A213, A269 or A312 where applicableSelect the standard according to heat-exchanger tube, general-service tubing or process pipe.
Europe1.4571 / X6CrNiMoTi17-12-2EN 10088 familyUse the product-specific EN dimensional and delivery standard.
Germany legacy referenceX6CrNiMoTi17-12-2DIN / Werkstoff 1.4571Legacy drawings should be translated into a current product specification.
SwedenSS 2350Legacy/national cross-referenceConfirm current acceptance against EN 1.4571 or the named project standard.
China06Cr17Ni12Mo2TiGB/T grade cross-referenceChinese designation and numbering are not identical to UNS S31635. Verify the grade, product standard and acceptance requirements before substitution.
“316Ti” is not a complete purchase specification. Specify the governing product standard and edition, grade designation, form, dimensions, finish, delivery condition and inspection documents. Corrosion tests or elevated-temperature design data should be requested when the service calls for them.

Use the steel grade equivalents chart for an initial cross-reference, then verify every substitution against the current standard and heat certificate.

Chemical Composition, Titanium Requirement and PREN

The alloy uses chromium, nickel and molybdenum for 316-family corrosion performance. Titanium preferentially combines with carbon and nitrogen. For ASTM UNS S31635 flat-product chemistry, titanium is specified relative to carbon plus nitrogen. Do not transfer that exact ratio to EN 1.4571 or a GB/T product without checking the governing standard and edition.

Common ASTM A240-type limits for UNS S31635, weight percent
ElementCommon limitWhy it matters
Carbon (C)≤ 0.080%Available carbon affects the amount of titanium required for stabilization.
Chromium (Cr)16.00–18.00%Supports passivity, oxidation resistance and PREN.
Nickel (Ni)10.00–14.00%Maintains the austenitic structure and supports forming and toughness.
Molybdenum (Mo)2.00–3.00%Improves resistance to chloride pitting and crevice corrosion.
Titanium (Ti)5 × (C + N) minimum; 0.70% maximum (ASTM S31635 reference)Forms titanium carbonitrides and reduces chromium-carbide sensitization.
Nitrogen (N)≤ 0.10%Contributes to strength and is included in the titanium stabilization relationship.
Manganese (Mn)≤ 2.00%Supports steelmaking and austenite balance.
Silicon (Si)≤ 0.75%Deoxidation and oxidation behavior.
Phosphorus / sulfurP ≤ 0.045%; S ≤ 0.030%Controlled residuals affecting hot work, cleanliness and corrosion behavior.

Standards boundary: the composition table above summarizes the ASTM/UNS S31635 flat-product reference, not an independent laboratory result. European 1.4571 and Chinese cross-references can have different chemistry limits, including titanium rules. Follow the standard edition in the purchase order and check the certified heat analysis. For standard coverage, see ASTM A240/A240M-26.

What titanium does

Titanium combines with carbon and nitrogen so less carbon is available to form chromium-depleted grain-boundary carbides.

What titanium does not do

It does not materially raise PREN, eliminate chloride SCC or guarantee seawater resistance.

What the MTC must show

Heat chemistry should permit verification of C, N and Ti against the required stabilization relationship.

A common first-pass pitting resistance calculation is PREN = Cr + 3.3Mo + 16N. Typical 316Ti chemistry normally gives a PREN in the low-to-mid 20s, broadly similar to 316 and 316L. Use the PREN calculator for grade screening, but do not use PREN alone as a seawater or chemical compatibility guarantee.

Mechanical and Physical Properties

Annealed 316Ti has mechanical properties close to standard Type 316. Actual acceptance values depend on product form, thickness, test direction, standard and heat treatment. Cold work increases strength and can reduce elongation.

Representative room-temperature properties for annealed 316Ti flat product
PropertyASTM A240-type minimum or maximumProcurement note
0.2% proof / yield strength≥ 205 MPaThickness and product standard can change the required value.
Tensile strength≥ 515 MPaDo not substitute typical mill data for the specified minimum.
Elongation≥ 40%Gauge length, orientation and thickness must match the standard.
Hardness95 HRB maximum in a published S31635 plate referenceConfirm the actual scale, limits and acceptance route in the purchase standard; do not assume universal equivalence across forms.
Representative physical properties of 316Ti
PropertyTypical valueDesign note
DensityAbout 8.00 g/cm³Use the metal weight calculator for preliminary quantity estimates.
Thermal conductivity at 100°CAbout 14.6 W/m·KLower than carbon steel; thermal gradients and distortion require control.
Mean thermal expansion, 20–100°CAbout 16.5 µm/m·°CAllow for expansion in hot piping and dissimilar-metal assemblies.
Magnetic responseNormally low when annealedCold work can increase local permeability.
Heat hardeningNot hardenable by heat treatmentStrength increases primarily through cold work, not quenching.

Titanium Stabilization, Service Temperature and Heat Treatment

Standard 316 can become sensitized when chromium carbides form at grain boundaries during exposure in an intermediate-temperature range. 316Ti is designed so titanium carbonitrides form preferentially, preserving chromium near the grain boundaries. This advantage depends on chemistry and thermal history.

Thermal issues that should be defined before specifying 316Ti
IssueWhy it mattersWhat to specify
Sensitizing exposureRepeated or prolonged exposure around roughly 425–815°C can change carbide precipitation behavior.Operating temperature, duration, cycles and corrosive medium.
Solution annealingHigh-temperature annealing dissolves prior precipitates and restores ductility, but cooling and subsequent stabilization matter.Required delivery heat treatment and product standard.
Stabilization treatmentAn intermediate heat treatment may be required to precipitate titanium carbides before lower-temperature service.Whether stabilization annealing and intergranular-corrosion testing are required.
Creep / stress ruptureStabilization is not the same as guaranteed high-temperature strength.Design code, allowable stress and certified elevated-temperature data.
Oxidation atmosphereMolybdenum-bearing alloys can behave poorly in some stagnant high-temperature oxidizing conditions.Gas chemistry, flow, condensation, maximum metal temperature and cycling.
Do not select 316Ti from temperature alone. A valid high-temperature selection must combine the corrosion medium, time at temperature, stress, thermal cycling, oxidation atmosphere and applicable pressure or equipment code.

Welding, Fabrication and Knife-Line Attack

316Ti is generally weldable by common austenitic stainless processes, but stabilized grades introduce details that should be covered by the WPS. Weld-metal selection, dilution, heat input, interpass temperature, copper or zinc contamination and post-weld surface restoration all influence reliability.

Key 316Ti welding and fabrication controls
Control pointRisk if omittedRecommended RFQ or fabrication detail
Filler metalIncorrect weld chemistry, cracking or reduced corrosion performance.State WPS/PQR and approved 316L-type or E318-type filler where applicable.
Heat input and interpass temperatureExcessive distortion, sensitization or undesirable HAZ microstructure.Qualified welding procedure and recorded heat input.
Knife-line attack reviewA narrow corrosion band can form beside a weld after later sensitizing exposure.Thermal history, service temperature and required corrosion test.
Heat-tint removalChromium-depleted oxide can lower local corrosion resistance.Pickling, mechanical cleaning and passivation acceptance.
Carbon-steel contaminationBrown staining and initiation sites after service.Dedicated tools, clean handling and final surface inspection.
Forming and gallingHigh forming load, pickup and surface damage.Tooling, lubrication, bend radius, springback and protective film.

If the component is a welded vessel operating mainly at moderate temperature, compare 316L rather than assuming 316Ti is always superior. If the component is designed for elevated-temperature strength, compare 316H and use the governing code’s allowable stresses.

Corrosion Resistance and Chloride Limits

Molybdenum gives 316Ti better pitting and crevice-corrosion resistance than 304-type stainless steel. Titanium mainly addresses sensitization; it does not create a higher chloride-alloy class. Temperature, deposits, crevices, aeration, residual stress and cleaning chemicals can dominate field performance.

Coastal atmosphere

May be considered after reviewing exposure, drainage, surface finish and maintenance; no general marine-life guarantee.

Continuous seawater

Not a default choice for warm, stagnant or crevice-rich immersion.

Hot chloride stress

Like other austenitic grades, it remains susceptible to chloride SCC.

Common service risks and material-selection responses
Service condition316Ti assessmentPossible next review
Food, beverage and mild process fluidsOften suitable if finish, cleaning and weld restoration are controlled.316L when low carbon and hygienic weld practice are the main requirements.
Coastal air and salt sprayBetter margin than 304, but maintenance and geometry remain important.2205 or higher alloy for severe deposits, high temperature or inaccessible cleaning.
Warm stagnant seawaterHigh localized-corrosion risk; not a default recommendation.2205, 2507 or a project-specific corrosion alloy.
Strong oxidizing nitric-acid serviceRequires separate review; Mo and Ti can be disadvantageous in some highly oxidizing tests.A grade selected from actual concentration and temperature data.
Hot chloride plus tensile stressSusceptible to chloride SCC despite titanium stabilization.Duplex stainless, nickel alloy or stress/temperature redesign.

Inspection, PMI and Traceability

A credible 316Ti order needs more than a stamped grade name. The inspection plan should prove alloy identity, stabilization chemistry, delivery condition, dimensions and any corrosion or elevated-temperature requirements.

Heat traceability

Match every sheet, plate, coil, pipe or bar bundle to the heat number and MTC.

Ti/C/N relationship

Check the certified carbon, nitrogen and titanium values against the required formula.

Delivery treatment

Confirm solution annealing, stabilization treatment or project-specific heat treatment.

Surface restoration

Inspect weld heat tint, iron contamination, finish, Ra and passivation where applicable.

Useful inspection methods and their limits
MethodUseful forImportant limitation
EN 10204 3.1 MTCHeat chemistry, mechanical properties, standard and heat treatment.Verify that markings and quantities genuinely trace to the certificate.
Handheld XRF PMIScreening Cr, Ni, Mo and often Ti with suitable equipment.Does not verify carbon or nitrogen and cannot alone prove the stabilization ratio.
OES / laboratory analysisMore complete chemistry including carbon and selected light elements.Sampling, calibration and acceptance criteria must be agreed.
Intergranular-corrosion testProject-specific assessment after sensitizing treatment.Practice and acceptance must match the actual alloy and service.
Dimensional / surface inspectionThickness, flatness, straightness, Ra, grain direction and defects.A finish name alone does not define cosmetic acceptance.

Typical 316Ti Applications

  • Chemical and petrochemical vessels, piping, columns and internals exposed to thermal cycling.
  • Heat exchangers, condenser components and hot process lines.
  • Refinery equipment, expansion components and furnace-adjacent fabricated parts.
  • Pulp, paper and sulfur-bearing process equipment where 316-type corrosion resistance is required.
  • Food or industrial equipment where a stabilized 316-family grade is specifically approved.
  • Fasteners, supports, bars and machined parts operating in corrosive elevated-temperature service.

The final selection should be based on actual chemical concentration, chloride level, temperature, time, stress, welding procedure and cleaning method. “High temperature” or “marine” alone is not a sufficient material specification.

For orders involving process piping, heat-exchanger tubing or other industrial tubular products, review XRTGSteel’s stainless steel pipe and tube purchasing page. Use the specified pipe or tube standard to confirm heat treatment, testing, dimensions and any code requirements.

316Ti vs 316L, 316H, 321, 347 and Duplex Stainless Steel

Selection-oriented comparison of 316Ti and adjacent grades
GradeDefining featureBest reason to select itMain caution
316Ti / S31635Titanium-stabilized 316 chemistry.Stabilized Mo-bearing alloy for specified hot corrosive service.Not inherently superior to 316L in chlorides or to 316H in creep strength.
316Standard-carbon Mo-bearing austenitic grade.General 316-family service where the standard grade is specified.Sensitization risk after unsuitable thermal exposure.
316LCarbon ≤ 0.030%.Welded tanks, pipework and hygienic equipment at moderate temperatures.Low carbon does not prevent all long-duration sensitization or chloride attack.
316HControlled higher carbon.Selected elevated-temperature strength and code applications.Corrosion and welding requirements need separate review.
321Titanium-stabilized 18Cr-8Ni without Mo.Stabilized hot service where 316-level pitting resistance is unnecessary.Lower chloride pitting resistance than 316Ti.
347Niobium-stabilized austenitic grade.Specified stabilized welding and elevated-temperature service.Different chemistry, filler and availability from 316Ti.
2205Duplex structure with higher Cr, Mo and N.Higher strength and better chloride/SCC resistance.Requires duplex-specific welding and heat-input control.

316Ti Product Forms, Photos and Processing

Representative stainless steel coil stock showing a possible processing form
Representative coil stock, not verified as 316Ti by appearance. For an actual order, confirm grade-specific availability, heat traceability, edge, finish, tolerance and delivery condition.
Representative stainless steel pipe and tube stock for industrial purchasing
Representative pipe and tube stock, not verified as 316Ti by appearance. Specify the standard, weld or seamless route, heat treatment, testing and service code separately from the grade.
Common 316Ti supply forms and processing options
Product or serviceTypical optionsKey RFQ detail
Sheet / plateCold-rolled sheet, hot-rolled plate, cut plate and protected sheet.Standard, thickness, tolerance, flatness, finish and heat treatment.
CoilNo.1, 2B, BA, slit edge and custom coil weight.Coil ID/OD, weight, edge, finish, film and MTC traceability.
StripNarrow strip, precision width and custom temper.Width tolerance, burr, camber, edge and mechanical condition.
Pipe / tubeSeamless, welded, process and heat-exchanger tube.ASTM/EN standard, OD, wall, weld route, heat treatment and NDT.
BarRound, flat, forged, peeled, turned or ground bar.Bar standard, tolerance, straightness, condition and machining allowance.
Cut-to-lengthCoil-to-sheet processing and leveling.Final size, squareness, flatness, protection and packing count.
SlittingWide coil to narrow strip.Width tolerance, burr, camber, edge condition and coil weight.
Surface finishingNo.4, hairline, polished or project-specific finish.Ra, cosmetic sample, grain direction, Ti-streak acceptance and film.
Laser cuttingBlanks, panels, brackets and drawing-based components.Drawing revision, tolerance, edge, heat tint and distortion acceptance.

Information Needed for an Accurate 316Ti Quotation

  • Grade and standard: S31635, Type 316Ti, EN 1.4571 or another explicitly approved designation.
  • Product form and size: sheet, plate, coil, strip, pipe, tube or bar with tolerances.
  • Thermal service: minimum/maximum temperature, time at temperature, cycles and atmosphere.
  • Corrosion service: chloride level, chemical concentration, pH, aeration, deposits and crevices.
  • Heat treatment: solution annealed, stabilization annealed or another project condition.
  • Welding: joint type, thickness, WPS/PQR, filler, post-weld cleaning and corrosion testing.
  • Inspection: required EN 10204 3.1 MTC, heat traceability, PMI and agreed C/N/Ti testing, IGC testing, dimensions, Ra or independent inspection as applicable.
  • Commercial details: quantity, destination, Incoterm, packaging and required delivery window.

Availability, mill route, MOQ, lead time, certificate scope and special testing must be reconfirmed for the exact grade, product standard and quantity. No unverified mill capacity or guaranteed tolerance is implied.

Practical Questions Buyers Ask About 316Ti

Can handheld XRF prove that material is 316Ti?

XRF can usually screen chromium, nickel, molybdenum and, with a suitable analyzer and calibration, titanium. It cannot verify carbon and nitrogen, while the stabilization requirement relates titanium to carbon plus nitrogen. Use the MTC and a suitable laboratory method when independent confirmation of S31635 or the titanium stabilization ratio is required.

What is the practical difference between 316Ti and 316L?

316L limits carbon to reduce sensitization during welding and short thermal cycles. 316Ti uses titanium to bind carbon and is selected when a stabilized 316-family grade is required for repeated or prolonged exposure in a sensitizing temperature range. Their basic molybdenum-assisted pitting resistance is broadly similar, so 316Ti is not automatically more corrosion resistant in chlorides.

Is 316Ti always better than 316L at high temperature?

No. The answer depends on temperature, exposure time, corrosion medium, pressure code and required creep strength. 316Ti addresses stabilization, while 316H may be selected for controlled higher-carbon elevated-temperature strength. The design code and certified elevated-temperature properties must govern the choice.

Can 316Ti stainless steel be welded?

Yes. It can be joined by common austenitic stainless welding processes. The WPS should control heat input, filler metal, interpass condition, contamination and post-weld cleaning. Depending on the procedure and code, low-carbon 316L-type or stabilized E318-type filler may be specified.

What is knife-line attack in a stabilized stainless steel?

Knife-line attack is a narrow band of intergranular corrosion close to a weld. It can occur if welding dissolves titanium carbides in a very small heat-affected zone and the component later spends time in a sensitizing temperature range before titanium carbides reform. It is a service- and thermal-history issue, not a defect that can be judged from the grade name alone.

Is 316Ti suitable for continuous seawater immersion?

It has better pitting resistance than 304 because it contains molybdenum, but it is not immune to warm, stagnant or crevice-rich seawater. Continuous seawater immersion, deposits and high chloride temperature often justify reviewing 2205, 2507 or another higher-alloy grade.

Is annealed 316Ti magnetic?

It is generally non-magnetic in the solution-annealed condition. Cold rolling, bending, drawing or machining can increase local magnetic response. Magnet attraction alone cannot confirm or reject the grade.

Why can polished 316Ti show streaks or small surface marks?

Surface appearance can be affected by mill quality, titanium-containing particles, grinding sequence, abrasive contamination, grain direction and protective-film handling. For visible or electropolished parts, approve a representative finish sample and specify Ra, defect limits and inspection lighting before production.

Technical sources and scope: ASTM A240/A240M-26 defines flat-product scope; the British Stainless Steel Association’s 316Ti comparison explains stabilization, welding and corrosion-selection limits. These references support general guidance, not a mill-specific material guarantee.

Technical review note: this page is a procurement and material-selection guide, not a substitute for the current material standard, pressure code, welding qualification, corrosion study or engineer approval. Final acceptance should follow the purchase specification and verified inspection documents.

Request a 316Ti Stainless Steel Quotation

Send the exact grade and product standard, dimensions, finish, quantity, heat-treatment condition, welding scope, operating temperature, corrosion medium, inspection requirements and destination. XRTGSteel can then check current stock, mill production, processing route, MOQ, packing and lead time for the actual requirement.

316Ti Datasheet Summary

Item316Ti
UNSS31635
EN number / name1.4571 / X6CrNiMoTi17-12-2
JISSUS316Ti
GB06Cr17Ni12Mo2Ti
StructureAustenitic, titanium-stabilized, molybdenum-bearing
Chromium (ASTM A240)16.0–18.0%
Nickel (ASTM A240)10.0–14.0%
Molybdenum (ASTM A240)2.00–3.00%
Carbon (ASTM A240)0.08% max
Titanium (ASTM A240)5 × (C + N) min, 0.70% max
Tensile / yield strength, min (ASTM A240)515 MPa / 205 MPa
Elongation, min (ASTM A240)40%
Hardness, max (ASTM A240)217 HBW / 95 HRB
PREN (Cr + 3.3Mo + 16N) from the A240 limitsabout 22.6–29.5, the same range as 316/316L

1.4571 vs 1.4404 (316Ti vs 316L) in European Specifications

In Europe the choice is usually between 1.4571 and 1.4404, not between ASTM grades. Both are covered by EN 10088. The main chemical differences in EN 10088-2 are shown below.

Element (%)1.4571 (X6CrNiMoTi17-12-2)1.4404 (X2CrNiMo17-12-2)
Carbon0.08 max0.030 max
Chromium16.5–18.516.5–18.5
Nickel10.5–13.510.0–13.0
Molybdenum2.00–2.502.00–2.50
Nitrogen—0.10 max
Titanium5 × C min, 0.70 max—
  • Both resist sensitization, by different routes. 1.4404 relies on very low carbon. 1.4571 relies on titanium binding carbon as titanium carbide. For normal welded fabrication, both are generally accepted.
  • Hot service: 1.4571 has traditionally been preferred in German-speaking markets for parts that spend long periods in the sensitizing temperature range, and for some pressure-equipment applications at elevated temperature.
  • Surface finish: titanium carbonitride particles can make a mirror or very fine polished finish harder to achieve on 1.4571. 1.4404 is usually chosen for bright decorative or hygienic polished surfaces.
  • Substitution: the two are not automatically interchangeable on a drawing. Get approval from the designer before replacing one with the other.

How Much Titanium Does 316Ti Need? A Worked Example

ASTM A240 requires titanium of at least 5 × (C + N). If a heat has 0.040% C and 0.012% N:

Minimum Ti = 5 × (0.040 + 0.012) = 0.26% (and no more than 0.70%).

Under EN 10088-2 (5 × C), the same heat would need at least 0.20% Ti. Check the mill test certificate for C, N and Ti and confirm the ratio is met. A certificate that lists Ti below the minimum, or no Ti at all, is not 316Ti.

Request a Quote Online 24/7/365

Scroll to Top

Contact Us

\n