347 stainless steel is a niobium-stabilized austenitic stainless steel. It is based on the 304 stainless steel family. Because it contains niobium, also called columbium in some standards, it gives strong resistance to intergranular corrosion after welding or thermal exposure.
This grade is widely used when welded parts must work at elevated temperatures. Niobium helps bind carbon and reduces chromium carbide precipitation at grain boundaries. Therefore, 347 stainless steel is useful for heat exchangers, refinery equipment, high-temperature piping, expansion joints and welded pressure equipment.
Compared with 304 stainless steel, 347 offers better stability after heat exposure. Compared with 321 stainless steel, 347 uses niobium stabilization instead of titanium stabilization. For higher creep strength, review 347H stainless steel.
XRTGSteel supplies 347 stainless steel in sheet, plate, coil, strip, pipe, tube and bar. In addition, we provide cut-to-length, slitting, laser cutting, surface finishing, polishing, sawing, welding support, testing support and export packing.
What Is 347 Stainless Steel?
Basic Grade Definition
347 stainless steel is a chromium-nickel austenitic stainless steel stabilized with niobium. It belongs to the 300 series stainless steel family. Its general corrosion resistance is close to 304, but its hot-service stability is stronger.
Main Performance Advantage
The main advantage of 347 is resistance to sensitization. Niobium combines with carbon and helps protect chromium at grain boundaries. As a result, 347 can resist intergranular corrosion in many welded and elevated-temperature conditions.
Typical Buying Reason
Buyers choose 347 when 304 or 304L is not stable enough after welding or repeated heat exposure. It is often used for refinery equipment, high-temperature piping, heat exchangers, boiler parts and aerospace exhaust components. However, chloride-rich or marine service may require a molybdenum-bearing grade such as 316L stainless steel.
Standards & Equivalent Grades of 347 Stainless Steel
International Grade References
347 stainless steel is available under many international standards. However, equivalent grades are not always exact matches. Therefore, the order standard, UNS number and mill test certificate should be checked before production.
| Country / Region | Standard | Grade / Designation |
|---|---|---|
| International | UNS | S34700 |
| USA | AISI / SAE | 347 |
| USA | ASTM A240 / A276 / A312 / A213 / A479 | Type 347 / TP347 |
| Europe | EN 10088 / EN 10095 | 1.4550 / X6CrNiNb18-10 |
| Japan | JIS G 4303 / G 4304 / G 4305 | SUS347 |
| China | GB Reference | 06Cr18Ni11Nb / 0Cr18Ni11Nb |
| UK Legacy | BS Reference | 347S17 / 347S31, depending on specification |
| Common Name | Market Name | SS 347 / Niobium-Stabilized Stainless Steel |
Ordering Note
347 should be ordered by product standard, product form, size, surface finish and required inspection documents. In addition, buyers should confirm whether 347 or 347H is required. This is important for high-temperature service, pressure piping and export projects.
More materials are listed in our stainless steel grades overview. You can compare 304L, 321, 347, 347H, 316L, 316Ti and 310S there.
Chemical Composition of 347 Stainless Steel
Main Alloy Design
347 stainless steel uses chromium, nickel and niobium. Chromium provides stainless corrosion resistance. Nickel supports the austenitic structure. Niobium stabilizes carbon and improves resistance to intergranular corrosion after heating.
| Element | Typical Content | Main Function |
|---|---|---|
| C | ≤ 0.080% | Controlled carbon level for stabilized austenitic performance. |
| Cr | 17.00 – 19.00% | Provides stainless corrosion resistance and oxidation resistance. |
| Ni | 9.00 – 13.00% | Supports austenite stability, ductility and toughness. |
| Nb + Ta | ≥ 10 × C, typically up to 1.00% | Stabilizes carbon and reduces chromium carbide precipitation. |
| Mn | ≤ 2.00% | Supports steelmaking control. |
| Si | ≤ 0.75 – 1.00% | Supports deoxidation and oxidation resistance. |
| P | ≤ 0.045% | Controlled residual element. |
| S | ≤ 0.030% | Controlled for ductility and surface quality. |
| N | ≤ 0.10%, when specified | Controlled to support stability and specification compliance. |
| Fe | Balance | Main base metal. |
Composition Check Before Order
Chemical limits can change by standard and product form. Therefore, final acceptance should follow the purchase standard and MTC. XRTGSteel can provide heat number, chemical analysis and mechanical test results for export orders.
Mechanical Properties of 347 Stainless Steel
Room-Temperature Properties
347 stainless steel offers good strength and ductility after solution annealing. Its room-temperature strength is close to 304 stainless steel. However, its main value is better stability in welded and elevated-temperature service.
| Product Form / Condition | Tensile Strength | Yield Strength | Elongation | Hardness |
|---|---|---|---|---|
| ASTM A240 sheet / plate, annealed | ≥ 515 MPa | ≥ 205 MPa | ≥ 40% | ≤ 201 HBW typical |
| EN 1.4550 sheet / plate, annealed | 500 – 700 MPa typical | ≥ 200 MPa typical | ≥ 40% typical | ≤ 215 HBW typical |
| Annealed coil / strip | 515 – 760 MPa typical | 205 – 350 MPa typical | 35 – 45% typical | Depends on temper |
| Pipe / tube | 515 – 760 MPa typical | 205 – 380 MPa typical | 35 – 45% typical | Depends on wall thickness |
| Round bar / flat bar | 515 – 780 MPa typical | 205 – 400 MPa typical | 30 – 45% typical | Depends on size and condition |
High-Temperature Property Note
347 stainless steel provides good strength and stability in many elevated-temperature applications. Still, allowable stress must follow the project code. For stronger creep performance, 347H or 321H should also be reviewed.
Physical Properties of 347 Stainless Steel
Typical Physical Data
The physical properties of 347 stainless steel are close to other 18/8 austenitic stainless steels. This grade is generally non-magnetic after solution annealing. However, slight magnetism may appear after cold work.
| Property | Typical Value |
|---|---|
| Density | About 7.90 – 8.00 g/cm³ |
| Melting Range | About 1400 – 1450°C |
| Elastic Modulus | About 190 – 200 GPa |
| Thermal Conductivity | About 16 W/m·K at 100°C |
| Electrical Resistivity | About 0.72 – 0.75 μΩ·m typical |
| Magnetism | Generally non-magnetic when annealed |
Practical Service Note
Physical data should not be used alone for material selection. Instead, temperature, atmosphere, chloride level, welding amount and thermal cycling should be reviewed together. This gives a safer basis for stainless steel selection.
Key Features of 347 Stainless Steel
Performance Highlights
347 stainless steel is chosen when 304-type corrosion resistance and strong stabilization are both needed. It has good weldability and formability. In addition, niobium stabilization helps protect welded parts after heat exposure.
Niobium Stabilization
Niobium helps bind carbon and reduce intergranular corrosion risk after heating.
High-Temperature Stability
347 performs better than standard 304 in many welded hot-service conditions.
Good Welded Performance
This grade is widely used for welded piping, pressure equipment and thermal assemblies.
Summary of Advantages
- Niobium-stabilized 18/8 austenitic stainless steel.
- Better resistance to intergranular corrosion after heat exposure than standard 304.
- Good stability in the 425–850°C carbide precipitation range.
- Good oxidation resistance in suitable elevated-temperature environments.
- Good weldability for pressure equipment, piping and fabricated assemblies.
- Good formability for sheet, plate, coil and strip products.
- Available as sheet, plate, coil, strip, pipe, tube and bar.
- Not designed for severe chloride or marine pitting service.
Heat Resistance, Weldability and Corrosion Resistance
Elevated-Temperature Service
347 stainless steel is widely used for parts exposed to welding heat or repeated thermal exposure. It performs well in many oxidizing high-temperature environments. However, the exact service limit depends on atmosphere, load, thermal cycling and exposure time.
Intergranular Corrosion Resistance
Niobium stabilization improves resistance to intergranular corrosion after welding or heating. This is useful when the material passes through the carbide precipitation range. Therefore, 347 is often selected for welded hot parts and thermal process equipment.
Welding and Forming
347 stainless steel can be welded by common stainless steel welding processes. However, filler selection, heat input control and post-weld cleaning are still important. For heavy welded structures in chloride service, 316L may be a better choice.
| Performance Item | 347 Stainless Steel Characteristics |
|---|---|
| General Corrosion Resistance | Good in many atmospheric, food, industrial and mild process environments. |
| Intergranular Corrosion Resistance | Very good after heat exposure because niobium stabilizes carbon. |
| High-Temperature Stability | Good to very good in many welded elevated-temperature applications. |
| Oxidation Resistance | Good in suitable oxidizing atmospheres, depending on temperature and service time. |
| Chloride Resistance | Similar to 304-type grades and lower than molybdenum-bearing 316L. |
| Weldability | Good with proper filler, heat input control and post-weld cleaning. |
| Heat Treatment | Not hardenable by quenching. Solution annealing restores ductility and corrosion resistance. |
For low-carbon general welded fabrication, compare 304L stainless steel. For titanium-stabilized hot service, review 321 stainless steel. For higher creep strength, compare 347H stainless steel. For chloride resistance, review 316L stainless steel.
Typical Applications of 347 Stainless Steel
Refinery and Petrochemical Equipment
347 stainless steel is widely used in refinery and petrochemical systems. Common parts include catalytic cracking units, process piping, manifolds, fittings and welded assemblies. The grade is useful where hot exposure and welding are both present.
Heat Exchangers and Boiler Components
Heat exchangers and boilers often need stable welded stainless steel. Therefore, 347 is used for heat exchanger tubes, superheater tubes, boiler parts and pressure components. The actual service temperature and code requirement should be checked before selection.
Aerospace and Exhaust Systems
Aerospace and exhaust systems use 347 for hot gas exposure and thermal cycling. Typical examples include aircraft exhaust manifolds, engine parts, expansion joints and thermal shields. Surface cleaning after fabrication helps maintain stainless performance.
- Heat exchangers, boilers, superheater tubes and high-temperature process equipment.
- Refinery equipment, petrochemical systems and catalytic cracking units.
- High-temperature piping, pipe fittings, flanges and welded assemblies.
- Expansion joints, bellows, thermal shields and furnace components.
- Aircraft exhaust manifolds, engine parts and aerospace components.
- Chemical processing equipment exposed to intermittent high temperatures.
- Food processing and sanitary equipment where post-weld corrosion resistance is required.
- Storage tanks, pressure vessels and industrial fabricated structures requiring stabilization.
347 vs 304L, 321, 347H, 316L, 316Ti, 309S and 310S Stainless Steel
Quick Comparison
Buyers often compare 347 with other heat-resistant or corrosion-resistant stainless steels. Each grade has a different balance of stabilization, corrosion resistance, hot strength and cost. Therefore, the service temperature and corrosion environment should guide the final choice.
| Grade | Main Advantage | Typical Use |
|---|---|---|
| 347 | Niobium-stabilized 304-type performance for welded hot service. | Refinery equipment, heat exchangers and high-temperature piping. |
| 304L | Low carbon and wide availability. | General welded fabrication and mild environments. |
| 321 | Titanium-stabilized austenitic stainless steel. | Exhaust systems, hot ducts and thermal equipment. |
| 347H | Higher carbon for improved creep strength. | More demanding high-temperature service and pressure parts. |
| 316L | Molybdenum improves chloride and pitting resistance. | Marine, chemical, food and pharmaceutical equipment. |
| 316Ti | Titanium stabilization plus molybdenum corrosion resistance. | Hot chemical service and 316-type stabilized equipment. |
| 309S | Higher chromium and nickel for stronger heat resistance. | Furnace parts, thermal shields and hot gas systems. |
| 310S | Excellent oxidation resistance in more severe heat service. | Radiant tubes, furnace liners and severe high-temperature parts. |
Selection Guidance
- Use 347 when niobium stabilization and welded hot-service performance are required.
- Select 304L when the environment is mild and low-carbon welded fabrication is enough.
- Choose 321 when titanium stabilization is specified or preferred.
- Choose 347H when higher creep strength is required in elevated-temperature service.
- Review 316L when chloride pitting resistance is more important than heat stabilization.
- Choose 316Ti when titanium stabilization and molybdenum-bearing corrosion resistance are both required.
- Review 309S or 310S when oxidation resistance at higher temperatures becomes the main requirement.
347 Stainless Steel Product Forms
Sheet, Plate and Coil
XRTGSteel supplies 347 sheet, plate and coil for hot-service and corrosion-resistant fabrication. These products can be cut, slit, polished or packed according to the order.
| Product Form | Available Options | Typical Use |
|---|---|---|
| 347 Sheet / Plate | Hot-rolled plate, cold-rolled sheet and cut plate. | Heat exchangers, tanks, pressure parts and fabricated equipment. |
| 347 Coil | No.1, 2B, BA, No.4 and custom coil weight. | Cut-to-length, slitting, formed parts and thermal fabrication. |
| 347 Strip | Narrow strip and custom width strip. | Bellows, clamps, heat shields, brackets and formed components. |
Pipe, Tube and Bar
Pipe, tube and bar are common choices for high-temperature piping and thermal equipment. For example, they are used in refinery systems, heat exchangers, fittings, supports and machined parts.
| Product Form | Available Options | Typical Use |
|---|---|---|
| 347 Pipe / Tube | Seamless pipe, welded pipe, process tube and heat exchanger tube. | Hot piping, refinery lines, heat exchangers and pressure systems. |
| 347 Bar | Round bar, flat bar, forged bar, angle and channel. | Fittings, fasteners, shafts, supports and machined hot-service parts. |
Processing and Testing Support
Processing Services
XRTGSteel can process 347 stainless steel before shipment. This helps buyers save time and control fabrication cost. Available services include cutting, slitting, surface finishing and sawing.
| Service | What We Provide |
|---|---|
| Cut-to-Length | Cut coil into sheets with required length and packing quantity. |
| Slitting | Slit coil into narrow strip for forming, bellows, exhaust parts and fabrication. |
| Surface Finishing | Supply No.1, 2B, BA, No.4, hairline and polished finishes. |
| Laser Cutting | Prepare panels, brackets, heat shields, blanks and custom parts. |
| Saw Cutting | Cut bar, pipe and tube to required length. |
| Welding Support | Support filler review, post-weld cleaning guidance and project document review. |
| Export Packing | Use waterproof paper, pallets, wooden cases and bundle protection. |
Inspection Support
For critical projects, we can coordinate PMI, tensile testing, hardness testing and third-party inspection. In addition, we can supply MTC documents, packing records and inspection reports.
How to Order 347 Stainless Steel from XRTGSteel
Information Needed for Quotation
A clear inquiry helps us quote faster. Please send the grade, size, quantity, surface finish and delivery destination. For hot-service projects, temperature and thermal cycling data are also important.
- Grade: 347, UNS S34700, 1.4550, SUS347 or project-specified equivalent.
- Product form: sheet, plate, coil, strip, pipe, tube, bar or custom part.
- Size: thickness, width, length, diameter or wall thickness.
- Surface finish: No.1, 2B, BA, No.4, hairline, polished or pickled.
- Processing: slitting, cutting, laser cutting, sawing or polishing.
- Service condition: temperature, atmosphere, thermal cycling, chloride level and exposure time.
- Welding requirement: tank welding, pipe welding, pressure welding or structural fabrication.
- Testing requirement: MTC, PMI, tensile test or third-party inspection.
- Quantity: pieces, kilograms, tons, coil weight or bundle quantity.
- Delivery term: FOB, CFR, CIF, DDP or other agreed Incoterms.
Material Selection Support
If the best grade is not clear, send your drawing and service condition. Our team can compare 347 with 304L, 321, 347H, 316L, 316Ti, 309S and 310S. Therefore, you can choose a safer material before ordering.
FAQ – 347 Stainless Steel
Q1: What is 347 stainless steel?
347 stainless steel is a niobium-stabilized austenitic stainless steel. It offers good corrosion resistance and better resistance to intergranular corrosion after welding or thermal exposure than standard 304. Therefore, it is widely used in refinery, heat exchanger, aerospace and high-temperature process equipment.
Q2: What is the UNS number of 347 stainless steel?
The UNS number is S34700. Common equivalent names include AISI 347, Type 347, TP347, EN 1.4550, X6CrNiNb18-10, SUS347 and 06Cr18Ni11Nb.
Q3: What is the difference between 304L and 347 stainless steel?
304L uses low carbon to reduce sensitization risk. 347 uses niobium stabilization. As a result, 347 is often better for long-term or repeated elevated-temperature exposure after welding.
Q4: What is the difference between 321 and 347 stainless steel?
Both grades are stabilized austenitic stainless steels. 321 is stabilized with titanium, while 347 is stabilized with niobium. Project standards, service temperature and welding requirements should guide the final selection.
Q5: Is 347 stainless steel suitable for high-temperature service?
Yes. 347 stainless steel is widely used for elevated-temperature service. It performs well in many welded hot-service conditions. However, atmosphere, load, exposure time and design code should be checked before final selection.
Q6: Can 347 stainless steel be welded?
Yes. 347 stainless steel has good weldability. Niobium stabilization helps protect the heat-affected zone after exposure to elevated temperature. Proper filler selection, heat input control and post-weld cleaning are still recommended.
Q7: Is 347 stainless steel good for marine environments?
347 has chloride resistance similar to 304-type stainless steels. It is not the best choice for severe marine or chloride pitting service. For chloride exposure, 316L, 2205 or a higher-alloy grade should be reviewed.
Q8: What 347 products can XRTGSteel supply?
XRTGSteel supplies 347 sheet, plate, coil, strip, pipe, tube and bar. We also provide cutting, slitting, finishing, sawing, welding support, testing support and export packing.
Request 347 Stainless Steel Price
Send your 347 stainless steel grade, product form, size, finish, quantity and destination port. XRTGSteel will help you confirm the right supply form and processing route.
For refinery, petrochemical, heat exchanger, boiler, aerospace, exhaust or high-temperature piping projects, please also send the service temperature, atmosphere, thermal cycling condition and testing requirement. This information helps us compare 347 with 304L, 321, 347H, 316L, 316Ti, 309S and 310S before quotation.