439 stainless steel is a titanium-stabilized ferritic stainless steel. It offers good weldability, good formability, strong oxidation resistance and better corrosion resistance than basic exhaust grades. It is widely used for automotive exhaust systems, heat exchangers, welded tubes, appliance parts, heat shields and formed thermal components.
The 17–19% chromium range gives 439 stainless steel better oxidation and corrosion resistance than 409 stainless steel. Titanium stabilization helps bind carbon and nitrogen. This improves weld stability and reduces the risk of intergranular corrosion after welding or thermal exposure.
Compared with 430 stainless steel, 439 stainless steel has better welded performance because of titanium stabilization. Compared with 441 stainless steel, 439 is often used when good exhaust performance is required but very high hot-end strength is not the main priority.
Compared with 304 stainless steel, 439 stainless steel is magnetic and usually more cost-effective because it has very low nickel content. However, 304 has better deep drawability and broader general corrosion resistance. For marine or chloride-rich service, 316L stainless steel should be reviewed.
XRTGSteel supplies 439 stainless steel in sheet, plate, coil, strip, welded tube, pipe, flat bar, round bar and custom-cut products. We also provide cut-to-length, slitting, surface finishing, laser cutting, plasma cutting, bending, roll forming, tube forming, welding support and export-grade packing.
What Is 439 Stainless Steel?
Basic Grade Definition
439 stainless steel is a titanium-stabilized ferritic stainless steel. It is not hardenable by heat treatment. It is magnetic in annealed, cold-worked, welded and fabricated conditions.
Main Performance Advantage
The main advantage of 439 is its balance of weldability, oxidation resistance and cost. It performs well in exhaust systems, welded tubes and thermal cycling parts. It is also useful when 409 is not durable enough and 304 is more expensive than required.
Typical Buying Reason
Buyers choose 439 when they need better exhaust durability, better weld stability and better corrosion resistance than 409. It is a practical option for mufflers, tailpipes, converter shells, heat exchangers, heat shields, welded tubes and appliance parts.
Standards & Equivalent Grades of 439 Stainless Steel
International Grade References
439 stainless steel is supplied under several international standards. Equivalent grades can vary by titanium requirement, carbon level, product form and order specification. Therefore, the final order should confirm the UNS number, EN designation, chemical limits and mill test certificate.
| Country / Region | Standard | Grade / Designation |
|---|---|---|
| International | UNS | S43035 |
| USA | AISI / SAE | 439 |
| USA | ASTM A240 / A268 / A554 / A480 | Type 439 / TP439 / S43035 |
| Europe / DIN | EN 10088 | 1.4510 / X3CrTi17 |
| Japan | JIS Common Reference | SUS439 |
| China | GB Reference | 022Cr18Ti / 00Cr18Ti, depending on specification |
| ISO | ISO Common Reference | X3CrTi17 / 439 family reference |
| Common Name | Market Name | SS 439 / 439 Stainless Steel / AISI 439 Stainless Steel |
Ordering Note
For exhaust systems, welded tubes, heat exchangers or formed parts, do not rely only on the grade name. Confirm the required standard, titanium stabilization, chemical limits, surface condition, thickness tolerance and inspection documents before production.
More materials are listed in our stainless steel grades overview. You can compare 439, 409, 409L, 430, 434, 436, 441, 444, 304 and 316L there.
Chemical Composition of 439 Stainless Steel
Main Alloy Design
439 stainless steel uses low-carbon chromium ferritic chemistry with titanium stabilization. Chromium improves corrosion resistance and oxidation resistance. Titanium improves welded performance by stabilizing carbon and nitrogen.
| Element | Typical Content | Main Function |
|---|---|---|
| C | ≤ 0.030 – 0.070%, depending on standard | Controlled to support weldability and ferritic stability. |
| Cr | 17.00 – 19.00% | Provides corrosion resistance, oxidation resistance and surface stability. |
| Ti | Stabilized, typically Ti ≥ 4 × (C + N) | Binds carbon and nitrogen to improve weld stability and thermal performance. |
| Mn | ≤ 1.00% | Supports steelmaking control. |
| Si | ≤ 1.00% | Supports deoxidation and oxidation resistance. |
| Ni | ≤ 0.50%, when specified | Usually low. Helps maintain ferritic structure and cost control. |
| N | ≤ 0.030 – 0.080%, depending on standard | Controlled with titanium for stability and weld performance. |
| P | ≤ 0.040% | Controlled residual element. |
| S | ≤ 0.030% | Controlled for ductility, weldability and surface quality. |
| Fe | Balance | Main base metal. |
Composition Check Before Order
Chemical limits can change by standard and product form. Therefore, final acceptance should follow the purchase standard and MTC. For welded tube, exhaust and thermal cycling projects, titanium stabilization should be checked carefully.
Mechanical Properties of 439 Stainless Steel
Annealed Sheet, Coil, Strip and Tube
439 stainless steel is commonly supplied in annealed sheet, coil, strip or welded tube condition. This condition supports bending, stamping, roll forming, tube forming and welding. Actual values depend on thickness, annealing condition, cold work level and testing direction.
| Condition / Product Form | Tensile Strength | Yield Strength | Elongation | Hardness |
|---|---|---|---|---|
| Annealed sheet / plate | 415 – 620 MPa typical | 205 – 345 MPa typical | 22 – 35% typical | ≤ 183 HBW typical |
| Annealed coil / strip | 420 – 600 MPa typical | 205 – 330 MPa typical | 22 – 36% typical | ≤ 89 HRB typical |
| Cold-worked strip | 550 – 850 MPa typical | 350 – 650 MPa typical | 8 – 25% typical | Higher, depending on temper |
| Welded tube / exhaust tube | 420 – 620 MPa typical | ≥ 205 MPa typical | Depends on tube size and process | Depends on forming and welding condition |
| Custom formed part | Project-specific | Project-specific | Project-specific | Controlled by drawing and fabrication route |
Mechanical Property Note
439 stainless steel is not hardenable by heat treatment. Strength can be increased by cold working. Annealing restores ductility, formability and fabrication performance.
Physical Properties of 439 Stainless Steel
Typical Physical Data
The physical properties of 439 stainless steel are typical for ferritic stainless steels. It has useful thermal conductivity compared with many austenitic grades. It is magnetic in common supply and service conditions.
| Property | Typical Value |
|---|---|
| Density | About 7.70 – 7.75 g/cm³ |
| Melting Range | About 1450 – 1510°C |
| Elastic Modulus | About 200 – 220 GPa |
| Thermal Conductivity | About 23 – 26 W/m·K at 100°C |
| Electrical Resistivity | About 0.60 μΩ·m typical |
| Magnetism | Magnetic in annealed, cold-worked and welded conditions |
Practical Service Note
Physical data should not be used alone for material selection. Instead, welding route, thermal cycling, oxidation exposure, corrosion condition, forming method and cost should be reviewed together. This gives a safer basis for selecting 439 stainless steel.
Key Features of 439 Stainless Steel
Performance Highlights
439 stainless steel is selected when welded ferritic stainless parts need better oxidation resistance and better durability than 409. It provides a useful balance of chromium content, titanium stabilization, formability and cost.
Titanium Stabilized
Titanium stabilization improves weld stability and reduces intergranular corrosion risk.
Better Than 409
Higher chromium improves oxidation resistance, corrosion resistance and appearance retention.
Economical Ferritic Grade
Low nickel content helps control cost compared with 304 and 316L stainless steel.
Summary of Advantages
- Titanium-stabilized ferritic stainless steel.
- Better oxidation resistance than 409 stainless steel in many exhaust applications.
- Better corrosion resistance and appearance retention than basic exhaust grades.
- Good resistance to intergranular corrosion after welding.
- Good formability for bending, stamping, roll forming and tube forming.
- Good thermal fatigue resistance for exhaust systems and heat-related components.
- Magnetic in annealed, cold-worked and welded conditions.
- Lower chloride resistance than molybdenum-bearing or austenitic stainless steels.
Weldability, Oxidation Resistance and Fabrication
Weldability
439 stainless steel has good weldability for a ferritic stainless steel. Titanium stabilization improves welded performance and helps reduce intergranular corrosion risk. Controlled heat input and proper post-weld cleaning are recommended.
Oxidation Resistance
439 offers good oxidation resistance in automotive exhaust, hot gas and moderate high-temperature air environments. It is often selected when 409 does not provide enough oxidation resistance or appearance retention.
Forming and Machining
439 can be roll formed, bent, stamped, drawn and tube formed in annealed condition. Machinability is fair to good with proper tooling and lubrication. Annealing can restore ductility after cold work.
| Performance Item | 439 Stainless Steel Characteristics |
|---|---|
| Weldability | Good for ferritic stainless steel. Titanium stabilization improves welded performance. |
| Oxidation Resistance | Good in exhaust gas, hot air and moderate thermal cycling environments. |
| Corrosion Resistance | Good for ferritic stainless service. Better than 409 in many exhaust and mildly corrosive applications. |
| Formability | Good for bending, stamping, roll forming, drawing and tube forming in annealed condition. |
| Machinability | Fair to good. Standard ferritic stainless tooling and suitable lubrication are recommended. |
| Heat Treatment | Not hardenable by quenching. Annealing improves ductility and reduces forming stress. |
| Surface Finish | Suitable for pickled, 2B, BA, brushed, polished and industrial finishes. |
For lower-cost exhaust applications, choose 409 stainless steel or 409L stainless steel. For better indoor appearance, choose 430 stainless steel. For molybdenum-enhanced pitting resistance, review 434 stainless steel or 444 stainless steel. For chloride-rich or marine environments, 316L stainless steel is usually more suitable.
Typical Applications of 439 Stainless Steel
Automotive Exhaust Systems
439 stainless steel is widely used for automotive exhaust systems. Common parts include mufflers, tailpipes, exhaust tubing, resonators, converter shells and exhaust manifolds. It offers better oxidation resistance and corrosion resistance than 409 in many cases.
Heat Exchangers and Thermal Equipment
Heat exchangers and thermal ducting often need weldability, oxidation resistance and thermal cycling stability. Therefore, 439 is used for heat exchangers, heat shields, hot gas ducting and formed high-temperature parts.
Appliance and Welded Tube Applications
439 is also used for appliance parts, washing machine components, dryer drums, welded tubes and roll-formed profiles. It is useful when magnetic stainless behavior, good welding and moderate corrosion resistance are required together.
- Automotive exhaust systems, mufflers, tailpipes, exhaust tubing and resonators.
- Catalytic converter shells, exhaust manifolds and hot-end exhaust components.
- Heat exchangers, heat shields, thermal ducting and high-temperature formed parts.
- Welded tubes, roll-formed profiles, conduits and formed stainless components.
- Water heaters, boilers, sugar industry equipment and mildly corrosive thermal systems.
- Appliance parts, washing machine components, dryer drums and household equipment.
- Kitchen equipment, catering equipment and food-service components in mild environments.
- Industrial fabrication requiring magnetic stainless steel with better performance than 409.
439 vs 409, 409L, 430, 434, 436, 441, 444, 304 and 316L Stainless Steel
Quick Comparison
Buyers often compare 439 with ferritic exhaust grades, molybdenum-bearing ferritic grades and austenitic stainless steels. Each grade has a different balance of cost, oxidation resistance, weldability, formability and corrosion resistance. Therefore, the final choice should follow the service temperature and corrosion exposure.
| Grade | Steel Type | Main Advantage | Typical Use |
|---|---|---|---|
| 439 | Titanium-stabilized ferritic stainless steel | Better oxidation, corrosion and weld stability than 409. | Exhaust systems, heat exchangers, welded tubes and appliances. |
| 409 | Titanium-stabilized ferritic stainless steel | Economical exhaust and heat resistance. | Mufflers, tailpipes, exhaust tubing and heat shields. |
| 409L | Low-carbon ferritic stainless steel | Low-cost exhaust performance and good welded tube stability. | Exhaust tubes, mufflers, tailpipes and welded thermal parts. |
| 430 | Ferritic 17Cr stainless steel | Good indoor appearance and moderate corrosion resistance. | Appliances, decorative panels and indoor structures. |
| 434 | Molybdenum-bearing ferritic stainless steel | Better pitting resistance than 430 due to molybdenum. | Automotive trim, outdoor parts and mild chloride service. |
| 436 | Mo + Nb stabilized ferritic stainless steel | Better ridging resistance and forming appearance than 430. | Automotive trim, visible exhaust parts and appliance panels. |
| 441 | Dual-stabilized ferritic stainless steel | Better high-temperature strength and thermal fatigue resistance. | Exhaust manifolds, converters and hot-end thermal parts. |
| 444 | Molybdenum-bearing stabilized ferritic stainless steel | Stronger chloride and pitting resistance than many ferritic grades. | Water heaters, tanks, heat exchangers and chloride-exposed parts. |
| 304 | Austenitic chromium-nickel stainless steel | Better deep formability, weldability and general corrosion resistance. | Tanks, food equipment, kitchen equipment and welded structures. |
| 316L | Austenitic molybdenum-bearing stainless steel | Much stronger chloride and chemical corrosion resistance. | Marine, chemical, food and pharmaceutical equipment. |
Selection Guidance
- Choose 439 when better oxidation resistance, corrosion resistance and weldability than 409 are required.
- Choose 409 or 409L when cost control is the main priority and basic exhaust performance is sufficient.
- Choose 430 when indoor appearance and general ferritic corrosion resistance are the main requirements.
- Choose 434 when molybdenum-enhanced pitting resistance is required in mild chloride environments.
- Choose 436 when better forming appearance and ridging resistance are required for visible parts.
- Choose 441 when high-temperature strength and hot-end exhaust durability are important.
- Choose 444 when stronger ferritic chloride resistance is required.
- Choose 304 or 316L when stronger formability, weldability or corrosion resistance is required.
439 Stainless Steel Product Forms
Sheet, Plate, Coil and Strip
XRTGSteel supplies 439 sheet, plate, coil and strip for exhaust systems, heat exchangers, appliances and thermal equipment. These products can be cut, slit, leveled, polished, brushed or protected with film according to the order.
| Product Form | Available Options | Typical Use |
|---|---|---|
| 439 Sheet / Plate | Hot-rolled plate, cold-rolled sheet, pickled sheet, 2B sheet and custom blanks. | Heat shields, converter shells, panels, brackets and thermal parts. |
| 439 Coil | No.1, 2B, BA, pickled, mill edge, slit edge and custom coil weight. | Exhaust tube production, cut-to-length processing and roll forming. |
| 439 Strip | Narrow strip, precision strip and custom width strip. | Muffler parts, heat shields, brackets, clamps and formed components. |
Pipe, Tube, Bar and Custom Products
439 pipe and tube are common choices for exhaust systems, heat exchangers and welded assemblies. Flat bar, round bar and custom blanks can be supplied for supports, brackets and fabricated industrial parts.
| Product Form | Available Options | Typical Use |
|---|---|---|
| 439 Pipe / Tube | Welded tube, exhaust tube, heat exchanger tube and custom cut tube. | Exhaust systems, heat exchangers, thermal ducting and welded assemblies. |
| 439 Flat / Round Bar | Flat bar, round bar, cut bar, machined bar and custom lengths. | Supports, brackets, frames and fabricated industrial parts. |
| 439 Custom Parts | Laser-cut blanks, formed parts, welded parts and semi-finished components. | Exhaust hardware, heat shields, converter shells and fabricated assemblies. |
Processing and Testing Support
Processing Services
XRTGSteel can process 439 stainless steel before shipment. This helps buyers save fabrication time and control production cost. Available services include cut-to-length, slitting, laser cutting, surface finishing, tube forming, bending and export packing.
| Service | What We Provide |
|---|---|
| Cut-to-Length | Cut coil into sheets or blanks with required length and packing quantity. |
| Slitting | Slit coil into narrow strip for exhaust parts, clamps and roll-formed parts. |
| Surface Finishing | Supply pickled, 2B, BA, brushed, polished and customized industrial finishes. |
| Laser Cutting | Prepare plates, sheets, blanks, brackets, heat shields and custom parts. |
| Plasma / Waterjet Cutting | Cut thicker plate and industrial blanks when required. |
| Tube Processing | Support welded tube forming, sizing, cutting, deburring and exhaust tube preparation. |
| Forming Support | Support bending, roll forming, stamping, tube forming and fabrication guidance. |
| Welding Support | Support ferritic stainless welding route review, heat input control and post-weld cleaning consultation. |
| Export Packing | Use waterproof paper, PVC film, steel frame, wooden pallet, wooden case and seaworthy packing. |
Inspection Support
For project orders, we can coordinate PMI, chemical analysis, tensile testing, hardness testing, thickness inspection, surface inspection and dimensional inspection. In addition, we can supply MTC documents, packing records and inspection reports.
How to Order 439 Stainless Steel from XRTGSteel
Information Needed for Quotation
A clear inquiry helps us quote faster. Please send the grade, product form, size, quantity, surface finish and delivery destination. For 439 stainless steel, titanium stabilization, thickness tolerance, welding use and thermal service are especially important.
- Grade: 439, UNS S43035, EN 1.4510, X3CrTi17, SUS439 or project-specified equivalent.
- Product form: sheet, plate, coil, strip, welded tube, exhaust tube, pipe, flat bar, round bar or custom blank.
- Size: thickness, width, length, diameter, wall thickness, bar size or strip tolerance.
- Condition: annealed, cold rolled, hot rolled, pickled, slit, leveled, formed or welded.
- Surface finish: No.1, 2B, BA, pickled, brushed, polished or custom industrial finish.
- Processing: cut-to-length, slitting, laser cutting, plasma cutting, waterjet cutting, bending, tube forming or welding support.
- Service condition: exhaust gas, thermal cycling, heat exchanger service, oxidation exposure or mild corrosion.
- Testing requirement: MTC, PMI, tensile test, hardness test, thickness report or surface inspection.
- Quantity: sheets, pieces, kilograms, tons, coil weight, strip coils, tube bundles or bar bundles.
- Delivery term: FOB, CFR, CIF, DDP or other agreed Incoterms.
Material Selection Support
If the best grade is not clear, send your drawing, welding method, forming route and service condition. Our team can compare 439 with 409, 409L, 430, 434, 436, 441, 444, 304 and 316L. Therefore, you can choose a safer material before ordering.
FAQ – 439 Stainless Steel
Q1: What is 439 stainless steel?
439 stainless steel is a titanium-stabilized ferritic stainless steel. It offers good weldability, good formability, good oxidation resistance and better corrosion resistance than 409 in many exhaust and thermal applications.
Q2: What is the UNS number of 439 stainless steel?
The UNS number is S43035. Common references include AISI 439, Type 439, TP439, EN 1.4510, X3CrTi17, SUS439 and 022Cr18Ti.
Q3: What is 439 stainless steel used for?
439 stainless steel is commonly used for automotive exhaust systems, mufflers, catalytic converter shells, exhaust tubing, heat exchangers, heat shields, appliance parts, welded tubes and formed thermal components.
Q4: What is the difference between 409 and 439 stainless steel?
439 stainless steel generally has higher chromium than 409. It normally provides better oxidation resistance, better corrosion resistance and better appearance retention. 409 is often more economical for basic exhaust applications.
Q5: What is the difference between 430 and 439 stainless steel?
430 stainless steel is a general 17Cr ferritic stainless steel. 439 stainless steel is titanium stabilized. This gives 439 better welded performance and better resistance to intergranular corrosion after welding.
Q6: Is 439 stainless steel corrosion resistant?
Yes. 439 stainless steel provides good corrosion resistance for ferritic stainless steel. It performs well in exhaust, thermal and mildly corrosive environments. It is not as chloride-resistant as 316L in marine or severe chemical service.
Q7: Can 439 stainless steel be hardened?
No. 439 stainless steel cannot be hardened by heat treatment. It can be strengthened by cold working. Annealing is used to restore ductility, formability and fabrication stability.
Q8: Is 439 stainless steel magnetic?
Yes. 439 stainless steel is ferritic and magnetic in annealed, cold-worked and welded conditions. This magnetic behavior is normal for ferritic stainless steel grades.
Q9: What 439 stainless steel products can XRTGSteel supply?
XRTGSteel supplies 439 stainless steel sheet, plate, coil, strip, welded tube, pipe, flat bar, round bar and custom-cut products. We also provide slitting, cut-to-length, polishing, laser cutting, plasma cutting, tube forming, bending, welding support and export packing.
Request 439 Stainless Steel Price
Send your 439 stainless steel grade, product form, size, surface finish, processing requirement, quantity and destination port. XRTGSteel will help you confirm the right supply form, titanium stabilization, surface condition, tolerance and packing option.
For automotive exhaust systems, mufflers, catalytic converter shells, exhaust tubing, heat exchangers, heat shields, appliance parts, welded tubes or formed thermal components, please also send the drawing, welding method, thickness tolerance and service temperature. This information helps us compare 439 with 409, 409L, 430, 434, 436, 441, 444, 304 and 316L before quotation.